Casting defects are the unwanted irregularities that appear in the casting during metal casting process. Casting process involves a number of variables and a loss of control in any of these variables can cause defects under certain circumstances. Some of the common defects, their features and remedies to prevent such defects are described below:
1. Porosity (Blow-holes and pin holes):
They appear as small holes in the casting. They may be open to surface (or) they may be below the surface of the casting. They are caused due to entrapped bubbles of gases. Molten metal absorb gases from various sources such as fluxes, moisture in sand , additives and normal atmosphere gasses and nitrogen. They may be causes by excessively hard ramming, improper venting, excessive moisture (or) lack of permeability in the sand.
Remedies:2. Shrinkage cavity:
Some times due to faulty design of casting consisting of very thick and thin sections, a shrinkage cavity may be caused at the junction of such sections. Shrinkage cavity is totally internal. It is illustrated in Fig., It is caused due to shrinkage of molten metal. It is sometimes called as 'Pipe'.
Remedies:3. Misrun:
This denotes incomplete filling of mould cavity. It may be caused by bleeding of molten metal at the parting of cope and drag, inadequate metal supply (or) improper design of gating.
Remedies:4. Cold shut:
A cold shut is formed within a casting, when molten metal from two different streams meets without complete fusion. Low pouring temperatures may be the primary cause of this defect.
Remedies:
5. Mismatch:
This defect takes place when the mould impression in the cope and drag do not sit exactly on one another but are shifted a little bit. This happens due to mismatch of the split pattern (dowel pin may have become loose) (or) due to defective clamping of cope and drag boxes.
Remedies:
6. Drop:
This happens when a portion of the mould sand falls into the molten metal. Loose sand inadequately rammed (or) lack of binder may cause this defect.
7. Scab:
This defect occur when a portion of the face of a mould lifts (or) breaks down and the recess is filled up by molten metal.
8. Hot tear:These cracks are caused in thin long sections of the casting, if the part of the casting cannot shrink freely on colling due to intervening sand being too tightly packed, offers resistance to such shrinking. The tear (or) crack usually takes place when the part is red hot and has not developed full strength, hence the defect is called "Hot Tear". Reason may be excessively tight ramming of sand.
Remedies:
9.Penetration:
When fluidity of liquid metal is high, it may be penetrated into the sand mould/core (into the voids between the sand particles) causing a fused aggregate of metal and sand on the surface of the casting leading to defect.
Remedies:
10.Sand wash:
Surface dip that results from erosion of the sand mold during pouring. This counter is formed in the surface of the final cast part.